The direct process, also called the direct synthesis, Rochow process, and Müller-Rochow process is the most common technology for preparing organosilicon compounds on an industrial scale. It was first reported independently by Eugene G. Rochow and Richard Müller in the 1940s.[1][2]
The process involves copper-catalyzed reactions of alkyl halides with elemental silicon, which take place in a fluidized bed reactor. Although theoretically possible with any alkyl halide, the best results in terms of selectivity and yield occur with chloromethane (CH3Cl). Typical conditions are 300 °C and 2–5 bar. These conditions allow for 90–98% conversion for silicon and 30–90% for chloromethane. Approximately 1.4 Mton of dimethyldichlorosilane (Me2SiCl2) is produced annually using this process.[3]
Few companies actually carry out the Rochow process, because of the complex technology and has high capital requirements. Since the silicon is crushed prior to reaction in a fluidized bed, the companies practicing this technology are referred to as silicon crushers.[4]